- Posts: 11
- Joined: Sat Apr 25, 2015 8:42 am
we're trying to connect a retention gap (~1m, desactivated, unpacked) to our PAH Select column (Agilent). Therefore I used a press fit made of glass. I put the two columns in MeOH, so that the polyimid-layer of the columns swell (heard that on a GC/MS Seminar) and then pushed them into the press fit. I plunged the whole thing into MeOH and rised the pressure to 3 bar, to look for bubbles and see if it sealed well. I tried it several times, but it didn't work. One time there were no bubbles, so i injected a PAH Standard, but the Retention times shifted and the resolution was bad. Next day i looked into the GC oven and the columns fell out of the press fit nearly by their own weight...
Does anybody have experience with press fits or has a good alternative for connecting columns?
By the way, does anybody have experience with the PAH Select column? The seperation of the PAH is pretty good, but after 15 injections of a PAH-Standard it started to tail badly...