- Posts: 21
- Joined: Wed Jul 18, 2012 7:55 pm
I could take the Carboxen 1006 out of the oven in order to condition the Molesieve 5A column at a higher temperature than 250 C but I'd rather not mess with the columns. Would I get sufficient conditioning of the Molesieve 5A column if I simply conditioned for several hours at 250 C as a compromise? How far/long could I push past the temperature limit of the Carboxen 1006 before it degrades?