I meet a trouble!each time I pack my DAC column 50*250 packed with RP C4 silica 300A! but because of this silica is very fragile, 750psi was used during packing !every time , the column efficiency is not well!including the plates and tailing factor!when I unpack the column ,I find that the column bed was not solidity at all ?how can I improve?